Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm

@Thickness 3.17 mm
0.0015 - 0.0025 in/in

@Thickness 0.125 in
Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Dry
Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Polymerization Shrinkage
Premix Premi-Glas® 1200H-20 Polyester SMC
Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec..
Linear Mold Shrinkage 0.0010 - 0.0025 cm/cm
0.0010 - 0.0025 in/in
Polymerization Shrinkage
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Polymerization Shrinkage
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass..
Linear Mold Shrinkage 0.0020 - 0.0025 cm/cm
0.0020 - 0.0025 in/in
ASTM D955
PolyOne Edgetek® AS-20GF-05GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0020 - 0.0025 cm/cm
0.0020 - 0.0025 in/in
ASTM D955
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0020 - 0.0025 cm/cm
0.0020 - 0.0025 in/in
ASTM D955
PolyOne Edgetek® BB-20GF/000 PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0010 - 0.0025 cm/cm
0.0010 - 0.0025 in/in
Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber
Heat stabilized, 50% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0010 - 0.0025 cm/cm
0.0010 - 0.0025 in/in
Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber
50% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Injection Molding; ISO 2577
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound
BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers.
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound
BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing ..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound
BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol..
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..
Linear Mold Shrinkage 0.0020 - 0.0025 cm/cm
0.0020 - 0.0025 in/in
ASTM D955
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0020 - 0.0025 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0025 in/in

@Thickness 0.125 in
ASTM D955
PolyOne Lubri-Tech™ MP-15MCF/15T-2S Modified PPO - 15% Milled Carbon Fiber - 15% PTFE - 2% Silicone  (disconti
Data provided by PolyOne.