Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF1030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber Heat stabilized 35% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB306G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | Injection Molding; ISO 2577 |
Vyncolit X7010 Novolac Phenolic Glass fiber reinforced molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek RB306G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced. Heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AR-37 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AW-17 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell BJ-37 Nylon 6, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell BR-17 Nylon 6, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 - 0.0050 cm/cm | 0.0035 - 0.0050 in/in | IS 13411-1992 |
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | LATI |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 - 0.0040 cm/cm | 0.0035 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® AM-10CF-20GF/000 HS Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram RamSter PF303G4 PBT, 20% Glass Fiber 20% Glass-fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |