Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00250 cm/cm Grade Count:10
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Linear Mold Shrinkage -0.00200 - 0.00400 cm/cm
-0.00200 - 0.00400 in/in
Average value: 0.00159 cm/cm Grade Count:11
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Linear Mold Shrinkage -0.00100 - 0.00400 cm/cm
-0.00100 - 0.00400 in/in
Average value: 0.000879 cm/cm Grade Count:42
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Linear Mold Shrinkage 0.000 - 0.00400 cm/cm
0.000 - 0.00400 in/in
Average value: 0.00126 cm/cm Grade Count:39
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Linear Mold Shrinkage 0.000100 - 0.00400 cm/cm
0.000100 - 0.00400 in/in
Average value: 0.00183 cm/cm Grade Count:6
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00240 cm/cm Grade Count:5
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Linear Mold Shrinkage 0.00200 - 0.00400 cm/cm
0.00200 - 0.00400 in/in
Average value: 0.00300 cm/cm Grade Count:7
Overview of materials for Phenolic, Novolac, Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.000200 - 0.00400 cm/cm
0.000200 - 0.00400 in/in
Average value: 0.000985 cm/cm Grade Count:19
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Linear Mold Shrinkage 0.000100 - 0.00400 cm/cm
0.000100 - 0.00400 in/in
Average value: 0.00150 cm/cm Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00333 cm/cm Grade Count:6
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00243 cm/cm Grade Count:5
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Linear Mold Shrinkage 0.00200 - 0.00400 cm/cm
0.00200 - 0.00400 in/in
ASTM D955
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy
High GlossInformation provided by Bhansali
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00204 cm/cm Grade Count:12
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00280 - 0.00400 cm/cm

@Temperature 80.0 - 80.0 °C
0.00280 - 0.00400 in/in

@Temperature 176 - 176 °F
Average value: 0.00304 cm/cm Grade Count:20
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Linear Mold Shrinkage 0.000500 - 0.00400 cm/cm
0.000500 - 0.00400 in/in
Average value: 0.00188 cm/cm Grade Count:28
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00225 cm/cm Grade Count:4
Overview of materials for Acrylic, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00240 cm/cm Grade Count:5
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage 0.00200 - 0.00400 cm/cm
0.00200 - 0.00400 in/in
ASTM D955
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy