Polymer Property : Linear Mold Shrinkage = 0.0150 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0150 - 0.0310 cm/cm
0.0150 - 0.0310 in/in
Average value: 0.0193 cm/cm Grade Count:6
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Linear Mold Shrinkage 0.0150 - 0.0500 cm/cm
0.0150 - 0.0500 in/in
Average value: 0.0219 cm/cm Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Linear Mold Shrinkage 0.0150 - 0.0200 cm/cm
0.0150 - 0.0200 in/in
Average value: 0.0175 cm/cm Grade Count:3
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.0150 - 0.0300 cm/cm
0.0150 - 0.0300 in/in
Average value: 0.0176 cm/cm Grade Count:6
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..