Physical Properties Metric English Comments
Linear Mold Shrinkage 0.018 - 0.026 cm/cm
0.018 - 0.026 in/in
ASTM D955
Kolon SPESIN® KP212VO Flame Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Linear Mold Shrinkage 0.018 - 0.026 cm/cm
0.018 - 0.026 in/in
Lehmann & Voss LUVOCOM® 80-8318-1 Polyacetal-copolymer, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Linear Mold Shrinkage 0.018 - 0.026 cm/cm
0.018 - 0.026 in/in
ASTM D955
Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin
Flame retardant, BLACKApplications: ConnectorsInformation provided by API-Kolon.
Linear Mold Shrinkage 0.018 - 0.026 cm/cm
0.018 - 0.026 in/in
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Linear Mold Shrinkage 0.018 - 0.026 cm/cm

@Thickness 3.20 mm
0.018 - 0.026 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.018 - 0.026 cm/cm

@Thickness 3.20 mm
0.018 - 0.026 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.018 - 0.026 cm/cm

@Thickness 3.20 mm
0.018 - 0.026 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.018 - 0.026 cm/cm

@Thickness 3.20 mm
0.018 - 0.026 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.018 - 0.026 cm/cm

@Thickness 3.20 mm
0.018 - 0.026 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.018 - 0.026 cm/cm

@Thickness 3.20 mm
0.018 - 0.026 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.016 - 0.026 cm/cm
0.016 - 0.026 in/in
ASTM D955
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer