Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ Electro 242-1 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ FFSL 7286/40 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 6010 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 6041 Liquid Silicone Rubber - Healthcare Radio Opaque (X-Ray Detectability) LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 8040 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2030 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2050 Liquid Silicon Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2060 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2530 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2631 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2651 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2671 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2752 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3285/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3485/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4030 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4640 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 7070 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT HE Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating - Physical Properties are subject to the substrate that is used. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 40 µm) PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 60 µm) PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/35 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM D955 |
Teknor Apex Monprene® MP-2315 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Silopren™ LSR 4060 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |