Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | Solvay Test |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1080-70 Polycarbonate Resin Description: LUPOY PC 1080-70 resin is designed for optical media discs applications. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Ch.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1200-03 Polycarbonate Resin Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 3010-22 Polycarbonate Resin Description: LUPOY PC 3010-22 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 3030-10 Polycarbonate Resin Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 3030-15 Polycarbonate Resin Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm | 0.00050 - 0.0025 in/in | |
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1201-22 Polycarbonate Resin Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1300-12 Polycarbonate Resin Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1303-07 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm | 0.00050 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm | 0.00050 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm | 0.00050 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm | 0.00050 - 0.0025 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGK5020 compound is a glass reinforced, flame retardant material. |