Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0023 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP BG004 SAN (Europe-Africa-Middle East)
LNP* LUBRICOMP* BG004 is a compound based on Styrene Acrylonitril resin containing Graphite. Added features include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow)
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
ISO 294-4, 2577
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
ISO 294-4, 2577
Lanxess Pocan® DP 2004 000000 PBT
PBT, non-reinforced, injection molding, halogen free flame retardant
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY
Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ..
Linear Mold Shrinkage, Flow 0.0023 cm/cm
0.0023 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Europe-Africa-Middle East)
LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber
Linear Mold Shrinkage, Flow 0.0023 - 0.0028 cm/cm

@Thickness 3.20 mm
0.0023 - 0.0028 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA
Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This ..
Linear Mold Shrinkage, Flow 0.0023 - 0.0043 cm/cm

@Time 86400 sec
0.0023 - 0.0043 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66
Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0023 cm/cm

@Thickness 2.00 mm
0.0023 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.0023 cm/cm

@Time 86400 sec
0.0023 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved