Polymer Property : Linear Mold Shrinkage, Flow = 0.0036 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.0036 - 0.0108 cm/cm
0.0036 - 0.0108 in/in
ISO 294-4
Solvay Technyl® A218GV33-BK 33% Glass Filled, Heat Stabilized, Hydrolysis Resistant, Black Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP ZX89743 PPE+PS (Europe-Africa-Middle East)
LNP* LUBRICOMP* ZX89743 is a compound based on PPE+PS Blend resin containing Glass Fiber, Glass Beads and a Proprietary Lubricant. Added features include : Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
ISO 204-4
DSM Akulon® Ultraflow K-FPG8 PA6-I-GF40
Glass Reinforced, High flow
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
60x60x2mm; ISO 294
BASF Ultradur B 4300 G6 High Speed Unc. 30% Glass Filled PBT
Ultradur B 4300 G6 High Speed Unc. is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap..
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Conditioned)
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan..
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry)
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan..
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
ISO 2577, 294-4
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
Linear Mold Shrinkage, Flow 0.0036 cm/cm
0.0036 in/in
ISO Data
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.