Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0035 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0035 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific) Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | ASTM D955 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | |
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | |
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | |
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Carbon fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | |
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | |
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0045 cm/cm | 0.0015 - 0.0045 in/in | |
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Laticonther 92 GR/65 PUR, 65% Graphite Reinforced High thermal conductivity product based on Polyurethane (PUR). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | |
LATI Latigloss 62 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 6 (PA6). Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Ameri.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL RN1300 PPE (Asia Pacific) 15% glass/mineral reinforced PPE. Nonchlorinated, nonbrominated, flame-retardant. Black and gray. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JF004ER PES (Europe-Africa-Middle East) LNP* Thermocomp* JF-1004 S-3 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JF004RXP PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004RXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JF004Z PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004Z is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: HV. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; E2P method |
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |