Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycolac® GRM2600L ABS High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific) LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | Compression molding; ISO 2577 |
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free
(discontinued **) Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0060 cm/cm | 0.0045 - 0.0060 in/in | |
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0080 cm/cm | 0.0045 - 0.0080 in/in | |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0060 cm/cm | 0.0045 - 0.0060 in/in | |
LATI Latiohm 63-08 PD02 G/25 PA6, 25% Glass Fiber Reinforced Dissipative product based on Polyamide 6 (PA6), impact modified. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO 294-4 |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0055 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0055 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm @Thickness 3.00 mm |
0.0045 - 0.0065 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm @Thickness 3.00 mm |
0.0045 - 0.0065 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® FR3009 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | Sim. To ISO 294-4 |
DSM Arnite® AV2 390 XT PET GF50 50% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | Sim. To ISO 294-4 |
DSM Arnite® AV2 370 XT PET-GF35 35% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0085 cm/cm | 0.0045 - 0.0085 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced Heat resistant grade with halogen-free flame retardant; applications include TV plug connectors and components in switchgear cabinets.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Polystyrol® 168 N Polystyrene (Europe) High molecular, heat-resistant grades used where high strength is required. Suitable for expanded film.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | TM=300°C, TW=80°C |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | TM=300°C, TW=80°C |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO 2577 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO 2577 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO 2577 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced General-purpose grade with 10% glass fiber for parts requiring especially good resistance to heat deformation.Applications: auto parts, steering-column cladding and water meters.Data was collected b.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Polystyrol® 143 EO Polystyrene (Europe) Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | Injection molding; ISO 2577 |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:.. |