Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0070 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS PC/ABS with high stiffness and impact performance |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm @Thickness 3.20 mm |
0.0070 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Thickness 3.20 mm |
0.0070 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® TE5000SZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 137050-02-03, 26062-94-2 and 103598-77-2Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | |
LATI Latilub 73/13-15T G/15 POM, 15% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Time 86400 sec |
0.0070 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Time 86400 sec |
0.0070 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE0049F PC LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding... |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.18 mm |
0.0070 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU) Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU) Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ASA 814 GY Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon DX92440 PC LNP STAT-KON* DX92440 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PC/ABS 830 SS7 BK Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RKN14 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RKN14 is a compound based on Nylon 66 resin containing Mineral, MOS2. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON CD000 PS (Europe-Africa-Middle East) LNP* Stat-kon* CD000 is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® PA6/6 03003 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP LNP* THERMOCOMP* MFB71L is a compound based on Polypropylene resin containing 35% Glass Bead, 5% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT1525-BK 15% Glass Fiber Reinforced, Impact Modified Nylon 6 Description: Glass Fiber Reinforced, Impact Modified Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF3820-N 38% Mineral/Glass Reinforced Developmental Grade Nylon 66 Description: Mineral/Glass Reinforced Developmental Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® 6357 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-0/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® LTG2623 Polycarbonate PreprocessingMax. Water content |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 20A Z PA12 Product Description: Grilamid L 20A Z is a medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20A Z is impact modified, hydrolysis-and heat stabilized. Grilamid L 20A Z is used for p.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® SK692FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | on Tensile Bar; E2P method |
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |