Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm | 0.0040 - 0.0090 in/in | Bergmann method; ASTM D955 |
PolyOne Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX1814N PC |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | SABIC Method |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
LATI Lasulf PSU Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | |
LATI Latistat 87/28-06 PC Dissipative product based on Polycarbonate (PC). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP ZI001 PPE+PS LNP* LUBRICOMP ZI001 is a compound based on PPE+PS resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RFB71S PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB71S is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | DIS 294-4 |
Wellman Wellamid® GF14-60 XE-NBK1 Nylon 6, 14% Glass Fiber Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1782-BK1 40% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | |
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.0090 cm/cm @Time 86400 sec |
0.0080 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.18 mm |
0.0070 - 0.0090 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |