Polymer Property : Linear Mold Shrinkage, Flow = 0.0105 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0080 - 0.0105 cm/cm
0.0080 - 0.0105 in/in
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Linear Mold Shrinkage, Flow 0.0103 - 0.0105 cm/cm

@Thickness 3.20 mm
0.0103 - 0.0105 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific)
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +..
Linear Mold Shrinkage, Flow 0.0075 - 0.0105 cm/cm
0.0075 - 0.0105 in/in
ISO DIS 294-4
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0065 - 0.0105 cm/cm
0.0065 - 0.0105 in/in
ISO DIS 294-4
Wellman Wellamid® GF1811-BK1 15% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0075 - 0.0105 cm/cm
0.0075 - 0.0105 in/in
ISO DIS 294-4
Wellman Wellamid® T512-BK 15% Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6
Description: Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0065 - 0.0105 cm/cm
0.0065 - 0.0105 in/in
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..