Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
PolyOne Maxxam™ PPH-40C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ASTM D955 |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
Polyplastic Armlen® PP MF 40-3M Polypropylene Copolymer, 40% Calcium Carbonate Injection moldingInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East) High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B6D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm @Thickness 3.20 mm |
0.0070 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.012 cm/cm @Thickness 3.20 mm |
0.0050 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HM3207SM PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, Good Weatherability, High ImpactApplication: Automotive Interior Parts CAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
LATI Latigray 88/10-01 CX/30 PEEK Radiopaque compound based on Polyetheretherketone (PEEK). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm @Thickness 3.20 mm |
0.0090 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm @Thickness 3.20 mm |
0.0090 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.012 cm/cm @Thickness 3.20 mm |
0.0030 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Asia Pacific) >PPE+PA66-I-TD10 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® GFT1835-WBK1 Nylon 66, 17% Glass Fiber Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on Tensile Bar; E2P method |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | on Tensile Bar, Flow; ISO 294 |
Eurostar Staramide BG3ST43 PA6, 15% Glass Fiber Filled, Impact Modified, Injection Molded BG3ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |