Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00800 - 0.0130 cm/cm | 0.00800 - 0.0130 in/in | Injection; ISO 2577 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |