Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne Maxxam™ MD 4245-1000 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ASTM D955 |
PolyOne Maxxam™ PPC-20C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.015 cm/cm @Thickness 3.20 mm |
0.014 - 0.015 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | |
LATI Latigray 52/11-01 CX/70 PP Homopolymer Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latishield 66-10A PA66, Steel Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.015 cm/cm | 0.0050 - 0.015 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Stat-kon ZX05043 PPE+PS (Europe-Africa-Middle East) LNP* Stat-kon* ZX05043 is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE, Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermotuf R1000IX2 PA6.6 (Europe-Africa-Middle East) LNP* THERMOTUF* R1000IX2 is a compound based on PA 66 resin, containing Impact Modifier. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf R1000IX4 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | annealed 130C 1hr; ASTM D955 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific) Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Thickness 3.20 mm |
0.013 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Thickness 3.20 mm |
0.013 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.0135 - 0.015 cm/cm | 0.0135 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® GS1684-WBK1 25% Glass Sphere Filled Nylon 66 Description: Glass Sphere Filled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1615-BK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide B28 PA6, Injection Molded Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BS6 PA6, 30% Glass Bead Filled, Injection Molded Staramide BS6 is a 30% Glass Bead Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Time 86400 sec |
0.013 - 0.015 in/in @Time 24.0 hour |
E2P method |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.015 cm/cm @Time 86400 sec |
0.0080 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re.. |