Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ASTM D955
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE)
Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora..
Linear Mold Shrinkage, Flow 0.016 - 0.033 cm/cm

@Thickness 3.17 mm
0.016 - 0.033 in/in

@Thickness 0.125 in
ASTM D955
Network Polymers Softflex® 0470
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4
Akro-Plastic Akromid® S31 (3484) PA 6.10 Conditioned  (discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Thickness 3.20 mm
0.016 - 0.018 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL EI5002L PP
Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Thickness 3.20 mm
0.016 - 0.018 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm
0.016 - 0.018 in/in
LATI Latene® 11 MDT05-01 PP Homopolymer
Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
1/8" Section
Lucent Polymers PPC-320 Polypropylene, Impact Modified
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Time 86400 sec
0.016 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON WS002I PBT (Asia Pacific)
LNP* Stat-kon* WS002I is a compound based on Polybutylene Terephalate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® POM CO GF5 CC 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 5% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Luriblend® HTN 05007
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, ..
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
SABIC Method
SABIC Innovative Plastics LNP Thermocomp M10009A PP (Europe-Africa-Middle East)
LNP* STARFLAM* M10009A is a compound based on Polypropylene resin, containing Flame Retardant. Added features include : Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East)
NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66
Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C..
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PBT 0150 S
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PBT 0158 S
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
24 hours
Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
DIS 294-4
Wellman Wellamid® NY1875-BK1 Nylon 66, Unfilled
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® AZ 3/2 PA66
Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE..
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 4.00 mm
0.016 in/in

@Thickness 0.157 in
E2P method
Eurostar Starflam M10009XP PP, Flame Retardant, Injection Molding
Starflam M10009XP is an Unfilled Flame Retardant Polypropylene (Copolymer) Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
Eurotec
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, heat stabilized, black
Information provided by Eurotec®
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
Eurotec
Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4
Barlog Plastics KEBAFORM C 906 UR POM Copolymer unreinforced, impact modified
POM-IInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4
Barlog Plastics KEBATER BM330 PBT, 30% mineral reinforced, good light reflection
PBT-MD30Information provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored
High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration..
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a..
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
1/8" Section
Lucent Polymers PPC-0222 Polypropylene, Impact Modified
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® 22LH-WBK Unfilled Nylon 66
Description: Unfilled Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ASTM D955
PolyOne Stat-Tech™ PP-CP1/000 HF6 Black Polypropylene Impact Copolymer (PP Impact Copolymer)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Copyright © lookpolymers.com All Rights Reserved