Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | ASTM D955 |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 3.17 mm |
0.012 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000MDL Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedForm: Pellets Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D955 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 1245D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Medium Modulus, Black colorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HG3100 PP+MF10%, High Gloss Description: Injection Molding, PP+MF10%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Latistat 52/7-02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm | 0.016 - 0.018 in/in | annealed 130C 1hr; ASTM D955 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ISO DIS 294-4 |
Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy Description: Nylon/Polypropylene AlloyInformation provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 4.00 mm |
0.012 - 0.018 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 4.00 mm |
0.016 - 0.018 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starflam PX07037 PA6, Flame Retardant, Injection Molded Starflam PX07037 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (IR laser marking grade)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 3.17 mm |
0.012 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000MD5L Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant (5%)Features: LubricatedForm: Pellets Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Later 4-V0 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L.. |