Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.025 - 0.028 cm/cm | 0.025 - 0.028 in/in | ASTM D955 |
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.027 cm/cm | 0.025 - 0.027 in/in | ASTM D955 |
PolyOne Edgetek® 5230 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.027 cm/cm | 0.025 - 0.027 in/in | |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.027 cm/cm | 0.025 - 0.027 in/in | |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KA000M POM (Europe-Africa-Middle East) LNP* LUBRICOMP* KA000M is a compound based on Acetal Copolymer resin containg Aramide and Proprietary Lubricant. Added features include Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.030 cm/cm @Time 86400 sec |
0.025 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.030 cm/cm @Time 86400 sec |
0.025 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRILOY UX98388 PPA LNP LUBRILOY* UX98388 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | |
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme.. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm @Thickness 3.17 mm |
0.025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PBT FR X Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.030 cm/cm | 0.025 - 0.030 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1867-BK1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | annealed; ISO 294-4 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.035 cm/cm @Time 86400 sec |
0.025 - 0.035 in/in @Time 24.0 hour |
|
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 55 A.01 TPE-S, Shore A55, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.025 cm/cm @Thickness 3.17 mm |
0.025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PBT FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |