Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE) Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9065 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9072 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9077 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9082 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9090 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9172 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9177 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9182 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynaflex™ G6713C Thermoplastic Elastomer (TPE) Dynaflex™ G6713C is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV Sta.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | 15.6°C; ASTM D4.52 |
ExxonMobil 100 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D1505 |
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel Product Description: Vistamaxx 3980FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | 15.6°C; ASTM D4.52 |
ExxonMobil 100 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Specific Gravity | 0.878 g/cc | 0.878 g/cc | ASTM D792 |
PolyOne Elastamax™ XL 0141-66 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |