Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4970 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4975 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4995 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® D6880 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® D6890 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® D6970 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® P2950T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4885 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® P3950CT TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® P3953CT TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1377A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR110MC2 is a metallocene random copolymer with a melt flow index of 110 g/10 min for injection molding. This Lumicene® MR110MC2 high fluidity differs from standard random copolymers by .. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total Lumicene® MR30MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding Lumicene® MR30MX0 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection and injection stretch blow molding. Lumicene® MR30MX0 differs from the other random copolyme.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total Lumicene® MR60MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR60MC2 is a metallocene random copolymer with a melt flow index of 60 g/10 min for injection molding. Lumicene® MR60MC2 differs from standard random copolymers by its molding reproducib.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R021 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | method B; ASTM D792 |
Amco PRIMATOP PP CO 005NB Fractional Melt Polypropylene Copolymer Features:heat aging resistanceimpact resistancelow temperature melt strengthgood stiffnessApplications:containerspipestoysextrusion coatingFormer A-Top Polymers product; part of Amco product line si.. |