Polymer Property : Specific Gravity = 0.936 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.936 g/cc
0.936 g/cc
ISO 1183
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene
Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug..
Specific Gravity 0.936 g/cc
0.936 g/cc
ISO 1183
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene
Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha..
Specific Gravity 0.936 g/cc
0.936 g/cc
ISO 1183
Polimeri Europa Clearflex® RM 50 U Linear Medium Density Polyethylene
Clearflex RM 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RM 50 U show good mecha..