Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.936 g/cc | 0.936 g/cc | ISO 1183 |
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug.. |
|||
Specific Gravity | 0.936 g/cc | 0.936 g/cc | ISO 1183 |
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Specific Gravity | 0.936 g/cc | 0.936 g/cc | ISO 1183 |
Polimeri Europa Clearflex® RM 50 U Linear Medium Density Polyethylene Clearflex RM 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RM 50 U show good mecha.. |