Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
Polymax® Maxelast® P1980 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Er.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MQ 70 High Density Polyethylene - Injection Molding Eraclene MQ 70 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MQ 70 is suggested in applications for which high creep, impact and .. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
Polymax® Maxelast® P2885 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and st.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommend.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Gree.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MQ 70 U High Density Polyethylene - Injection Molding Eraclene MQ 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a mediu.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D1505 |
LG Chemical LUTENE-H ME5000 HDPE Description: LUTENE-H ME5000 is mainly intended for injection molding of containers and bottle cap. It has good stress cracking resistance and high impact strength.Applications: Containers, dust bin.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D1505 |
LG Chemical LUTENE-H PE0235 HDPE Description: LUTENE-H PE0235 is a materials with high toughness and rigidity suitable for cable protection It has very high resistance to stress cracking and long-term internal pressure creep proper.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM 792 |
Multibase Multi-Flex® D 6505 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInform.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM 792 |
Multibase Multi-Flex® RP 6568 B2 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM 792 |
Multibase Multi-Flex® A 5500 MR Natural TPE Thermoplastic Elastomer Information provided by Multibase |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ H2001WC High Density Polyethylene Wire & Cable Grade Key Characteristics:Excellent environmental stress cracking resistance (ESCR), high mechanical properties, high speed extrusionRecommended Applications:Jacketing of fiber optical cablesJacketing of .. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Total HDPE 56020 S High Density Polyethylene - Blow Molding HDPE 56020 S is a very high molecular weight (VHMW) high density polyethylene with a high resistance to impact, good chemical resistance and optimized balance between Environmental Stress Crack Resi.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding Lumicene® mPE M 5220 is a high density polyethylene with outstanding organoleptic properties, stress-cracking resistance and processability.Lumicene® mPE M 5220 is especially suited for the produc.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene This product is a Total Ecosolutions grade.Lumicene® mPE M5220M is a second generation metallocene high density polyethylene with very good organoleptic properties, dimensional stability, stress-cr.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene This product is a Total Ecosolutions grade.Lumicene® mPE M 5220 is a High Density Polyethylene with very good organoleptic properties, dimensional stability, stress-cracking resistance, rigidity an.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ISO 1183 |
Total HDPE 56020 S XP High Density Polyethylene - Blow Molding HDPE 56020 S XP is a very high molecular weight (VHMW) high density polyethylene with a high resistance to impact, good chemical resistance and optimized balance between Environmental Stress Crack R.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D1505 |
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding This hexene copolymer is tailored for injection molded applications that require:Excellent flowModerate impact strengthGood stiffnessTypical injection molded applications for 9035 include items such.. |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D792 |
Entec Hypel® PEHD30/.950 HDPE Available in North America Features: High DensityRoHS Compliant Form: Pellets Information provided by Entec |
|||
Specific Gravity | 0.952 g/cc @Temperature 25.0 °C |
0.952 g/cc @Temperature 77.0 °F |
|
Dow Corning 20 Demethiconol Blend A unique blend of silicone gum (6%) in dimethicone for use in a wide range of skin care and topical pharmaceutical applications.Information provided by Dow Corning |
|||
Specific Gravity | 0.952 g/cc | 0.952 g/cc | ASTM D1505/D792 |
Braskem Green PE SGM9450F Blow Film Extrusion and Cast Film Extrusion High Density Polyethylene Description: SGM9450F is a high-density polyethylene, developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tena.. |
|||
Specific Gravity | 0.952 - 0.960 g/cc | 0.952 - 0.960 g/cc | ASTM D792 |
Ravago Manufacturing Americas Echo® RPEHD BK HDPE Available in North AmericaDescription: Fractional Melt Recycled Content: Yes Color: Black Form: Pellets Information provided by Entec |