Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.960 - 1.00 g/cc | 0.960 - 1.00 g/cc | ASTM D1505 |
S&E Specialty Polymers GPP1001V0M-HCO-15 PP Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high lev.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 281-45MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183 |
Solvay Engineered Polymers SEQUEL® 1492 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1492 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | |
Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet Maplon Catalog No. L050-C001K0101 is an extremely opaque white sheet. Sheet surface is smoothly embossed with similar finish on both sides..Main advantages: High opacity, High rigidity high thermal .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D297 |
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D297 |
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
Michelman® Michem® Emulsion 91735 Nonionic polypropylene emulsion Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 91735 is a sizing polymer for fiberglass and other fibers used to reinforce polypropylene.We serve many markets through MichemÂ.. |
|||
Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
Michelman® Resisto Coat™ 39AF Abrasion resistance coating Description: Abrasion resistance coatingUsage: Resisto Coat™ 39AF provides excellent, economical abrasion protection. It is used throughout the appliance industry as a protective finish on corn.. |
|||
Specific Gravity | 0.960 g/cc @Temperature 22.8 °C |
0.960 g/cc @Temperature 73.0 °F |
ASTM D792 |
Spartech PP5410 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
Teknor Apex Synres® PP G10 17 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7010-87 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D 792 |
Zylog Neoplast® 180 FT EB Thermoplastic Vulcanizate Neoplast 180 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183 |
Total HDPE HD 6081 High Density Polyethylene - Injection Molding HD 6081 is a high density polyethylene with very good organoleptic properties, rigidity and processability.It is especially suited for the production of caps & closures for non-carbonated drinks by .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Specific Gravity | 0.960 g/cc @Temperature 25.0 °C |
0.960 g/cc @Temperature 77.0 °F |
|
Dow Corning 9040 Silicone Elastomer Blend A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, haircare, color cosmetics, suncare, antiperspirants and deodorants, and w.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | |
Dow Corning 9-6346 SILANE 72% solids quaternary ammonium functional alkoxysilane, provides anti-static properties.Information provided by Dow Corning |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 and ISO 1183 |
ExxonMobil Santoprene® 691-73W175 Thermoplastic Vulcanizate Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for thin wall, architectural glazing and sealing applic.. |
|||
Specific Gravity | 0.960 g/cc @Temperature 25.0 °C |
0.960 g/cc @Temperature 77.0 °F |
|
Dow Corning 1501 Fluid A blend of an ultrahigh viscosity dimethiconol in cyclopentasiloxane for use in skincare, woundcare, scar therapy, suncare, haircare, antiperspirant and deodorant, and color cosmetic applications.In.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 2782 |
AlphaGary Evoprene™ GC 5651 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | Part B; TM R050-16 |
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |