Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.980 g/cc | 0.980 g/cc | 23/23°C; ASTM D792 |
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.980 - 1.02 g/cc | 0.980 - 1.02 g/cc | ASTM D792 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® DigiPrime® 2500 Primer Description: Primer for digital printing suitable for paper substratesUsage: DigiPrime® 2500 is a product that can be added to size press treatments or pigment coatings to optimize substrates for.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Emulsion 65140 Nonionic polypropylene emulsion Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 65140 is best used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is n.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Prime 4990R Ethylene acrylic acid dispersion Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4990R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent r.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Shin-Etsu Silicones KF-6040 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Teknor Apex Synres® PP G15 18 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7010-50D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 1002 Nitrile Elastomer Nipol 1002 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.The original medium.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 1042 Nitrile Elastomer Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is .. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 33-5SR Nitrile Elastomer Special-purpose, intermediate-viscosity nitrile rubber designed to provide maximum processing safety without fouling molds. Recommended for high-temperature injection molding of parts.Special purpos.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 0.980 g/cc @Temperature 25.0 °C |
0.980 g/cc @Temperature 77.0 °F |
|
Dow Corning BY 11-030 Silicone Surfactant A clear dispersion of a high molecular weight silicone surfactant in cyclopentasiloxane for use in skincare, suncare, shower gel, and color cosmetic applications. INCI Name: Cyclopentasiloxane (and).. |
|||
Specific Gravity | 0.980 - 0.990 g/cc @Temperature 25.0 °C |
0.980 - 0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 1896 FR KIT Two-part, translucent, heat cure.Information provided by Dow Corning |
|||
Specific Gravity | 0.980 g/cc @Temperature 25.0 °C |
0.980 g/cc @Temperature 77.0 °F |
|
Dow Corning Z-6228 SILANE Dow Corning® Z-6228 Silane is a dialkyldimethoxysilane. Silanes and siloxanes have been used for some time in this application to increase yield and improve the stereoregularity of the polyolefin r.. |
|||
Specific Gravity | 0.980 - 1.01 g/cc @Temperature 25.0 °C |
0.980 - 1.01 g/cc @Temperature 77.0 °F |
|
Dow Corning EG-3000 THIXOTROPIC GEL PARTS A&B Two-part, heat cure, thixotropic gel.Information provided by Dow Corning |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® GFPP 2010 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® DN601 Liquid Nitrile Elastomer Nipol DN 601 is a developmental liquid copolymer of butadiene and acrylonitrile containing reactive carboxyl groups. This polyme ris suggested for resin modification in adhesives and coatings.Carbox.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ISO 1183 |
Solvay Engineered Polymers DEXFLEX® 900 TPO
(discontinued **) Description: DEXFLEX® 900 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paint.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Lucent Polymers TPO-10T Thermoplastic Polyolefin, 10% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | Part B; TM R050-16 |
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |