Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.01 g/cc | 1.01 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Polymax® Maxelast® A9930 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Ovation Polymers SOFTAPLAS™ S 65A Thermoplastic Elastomer Thermoplastic Elastomer – Excellent hydrolytic Stability and balance of properties. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are p.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Network Polymers SBS 1000 Clear Styrene Butadiene Copolymer Description: Clear Styrene Butadiene CopolymerInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 1.01 - 1.31 g/cc | 1.01 - 1.31 g/cc | |
Parker Chomerics CHO-SHIELD® 610 A/B Conductive Epoxy Paint Highly Conductive Epoxy Paint. This is a two-component, silver plated, copper-filled, highly conductive epoxy paint. This coating was developed for application to non-conductive plastic substrates t.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific) Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SPE and NISPE confiations. Flame retardant performance capable of m.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Teknor Apex Tekbond® TB 1413A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 4855A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-4001A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene Information provided by A. Schulman. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Zeon Chemicals Zeonex® 480R Cyclo-Olefin Polymer |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
Zeon Chemicals Zeonex® 690R Cyclo-Olefin Polymer |
|||
Specific Gravity | 1.01 g/cc @Temperature 25.0 °C |
1.01 g/cc @Temperature 77.0 °F |
|
Dow Corning 808 RESIN Medium-soft, silicone resin binder for heat resistant maintenance paints and colored baking enamels.Information provided by Dow Corning |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D-792 |
Chevron Phillips K-Resin® XK44 SBC K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Thermoformed clam shell packagingThermoformed blister packsThermoformed medical traysBlow molded productsFeatures:Good clarityGood stiffnessGo.. |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | 23°C; ASTM D792 |
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |
|||
Specific Gravity | 1.01 g/cc @Temperature 25.0 °C |
1.01 g/cc @Temperature 77.0 °F |
|
Dow Corning 2-3900 Antifoam Compound 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Dow VORANOL™ CP 3131 Polyol VORANOL™ CP 3131 polyol is a low to medium reactivity polyether triol, especially designed for the production of hot molded polyurethane flexible foams.Information provided by Dow |
|||
Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Specific Gravity | 1.01 - 1.08 g/cc | 1.01 - 1.08 g/cc | ASTM D792 |
Buckeye Polymers BP RPPC 1720 TURXF Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |