Physical Properties Metric English Comments
Specific Gravity 1.283 g/cc
1.283 g/cc
ISO 1183
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers
PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized
Specific Gravity 1.283 g/cc
1.283 g/cc
Hexcel® HexPly® F522 Epoxy Resin
HexPly® F522 is an advanced, modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness, excellent hot-wet properties ..