Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.36 g/cc @Temperature 22.8 °C |
1.36 g/cc @Temperature 73.0 °F |
ASTM D792 |
Quadrant EPP KETRON® MD PEEK, A Metal-Detectable Polyetheretherketone |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R353AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-0951 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 50-1396 Polycarbonate, with carbon fiber, glass fiber and PTFE, electrically conducting Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
Loxim 330 01HB Nylon 6 Information provided by Loxim Industries |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1/CF/30/TF/13/SI/2/BK Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Specific Gravity | 1.36 g/cc @Temperature 23.0 °C |
1.36 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose) Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | |
Sylvin Technologies 9950-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
Techmer ES Plaslube® J-50/10/TF/15 BK223 Polycarbonate |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
Styron EMERGEâ„¢ 4202-8 MFR Polycarbonate EMERGEâ„¢ PC 4202-8 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. Ap.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SPF 4520 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Stiffness Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Lattice Green 30155U Concentrate Based In LLDPE DescriptionPOLYBATCH® 30155U is a green color concentrate containing an optimized blend of color and UV stabilizer based in LDPE. This concentrate was designed to provide color and UV stability in.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 MK30HI 30% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | Part A |
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
Colorite Polymers CS1533UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D-792 |
Axiall 3605 Rigid PVC, Extrusion, Natural Georgia Gulf 3605 is a special purpose compound formulated for the extrusion of thin wall profiles such as edge banding and furniture trim.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 2192 Wire & Cable Flexible PVC Non-lead stabilized SJTO, SJTOO oil resistant flexible cord jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom VN-051090 PVC Compound Compuestos Dominicanos SA manufactures polycom VN product series for the extrusion of printable sheets and banners providing excellent stability, ease of processing and excellent printable character.. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
PolyOne Edgetek® MLS-20GF/000 Polysulfone Alloy - 20% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | ASTM D 792 |
Karina 837-10/37-A-ERYB-LMP White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |
|||
Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |