Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Nylene® Vexel™ B12GF15 , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 is a 15% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Network Polymers Kepital® F10-02 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Technetics Group Amicon™ PEEK 30% Carbon
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Ensinger Sintimid™ V 15% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin Improved acid resistance. Applications: Products for improved chemical resistance. Information provided by API-Kolon. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Kolon KOCETAL® K100 Standard Grade Acetal Resin Suitable for extrusion and injection molding of thick products. Applications: Extruded use such as rod, pipe, tube, and sheetInformation provided by API Kolon. |
|||
Specific Gravity | 1.41 - 1.47 g/cc | 1.41 - 1.47 g/cc | ASTM D 792 |
Karina E 800-35/1-B-ERB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7980 PEEK, with carbon fiber Applications: medical engineeringHigh-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flamm.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® DR51 PBT 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON JX89626 PES LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
A. Schulman Aqualoy® 645 Glass Fiber Reinforced Hydrolysis Resistant Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE POLYBATCH™ Birch 60171U/4 is a birch color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability in p.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-17036 Glass Fiber Reinforced High Heat Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
A. Schulman PAPERMATCH® T-39617 Specialty Masterbatch DescriptionPAPERMATCH® T-39617 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. This masterbatch is a white, medium opacity grade with a smooth surface .. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D-792 |
Axiall 8266 Rigid PVC, Extrusion, White Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | "A" component |
ACC QSil 550R QSI Quantum Silicones Silicone Potting Material QSil 550Ris a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |