Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D792 |
S&E Specialty Polymers G-4785E PVC Application: Flexible, PVC material designed for general-purpose extrusion applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.44 g/cc @Temperature 22.8 °C |
1.44 g/cc @Temperature 73.0 °F |
ASTM D792 |
Quadrant EPP Ketron® CM HPV PEEK (1331) Compression Molded High Pressure Velocity Polyetherether Ketone |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R148AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E-844-10/219-Y-ERYM White PVC Compound Tin stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.I.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Lucent Polymers GPCB-330 Polycarbonate+PBT, 30% Glass Fiber Reinforced, Impact Resistant Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 704-35/1-J-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.50 g/cc | 1.44 - 1.50 g/cc | ASTM D 792 |
Karina E 813-18/190-Y-RT-PO Gray PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFI12 Acetal Copolymer LNP LUBRICOMP* KFI12 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Saint-Gobain Meldin® 3130 Thermoplastic Bearing Material Meldin 3130 components provide good strength and stiffness in addition to excellent high velocity performance. This formulation can be used with both hard or soft mating surfaces. Meldin® 3100 .. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SSG 7006 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST4; ST5; Type 6; YM1; YM2; TM2 Agency Ratings: BS 6746; IEC 60227; VDE 0207 For.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Light Grey 80426U Concentrate Based In LLDPE DescriptionPOLYBATCH® 80426U is a grey color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability in.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D-792 |
Axiall PURGOVIN® 8000 Rigid PVC, Extrusion Georgia Gulf PURGOVIN® 8000 is a unique vinyl based PVC pellet purging compound designed for use in the shutdown or cleaning of extrusion lines, blow molding machines, and injection molding machine.. |
|||
Specific Gravity | 1.44 - 1.48 g/cc | 1.44 - 1.48 g/cc | ASTM D-792 |
Axiall 19890 Wire & Cable Flexible PVC Highly recommended for 105°C, 15 mil wall insulations and jackets where good gasoline and oil resistance is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |