Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.32 - 1.45 g/cc | 1.32 - 1.45 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i.. |
|||
Specific Gravity | 0.950 - 1.45 g/cc | 0.950 - 1.45 g/cc | ASTM D792 |
Parker Chomerics Tecknit SC-Consil® 864 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP313 Cotton Fabric Description: Canvas phenolic laminate with molybdenum disulfide lubricant. Mechanical properties slightly lower than NP310.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP315 Cotton Fabric Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should .. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP322 Cotton Fabric Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320.. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP325 Cotton Fabric Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500". |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP347 Cotton Fabric Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1.. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP610 Paper Base Laminate Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne.. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP639 Paper Base Laminate Description: Economical paper reinforced laminate developed with capacity to withstand temperatures to 150° C without blistering. High compressive strength and low moisture absorption.Thickness T.. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina 809D10/161-BY-IS White PVC Compound PVC compound recommended for extrusion of forniture profile and flexible laminated.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 680D48/1-G-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 811-10/184-Y-CR White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 830-35/1-Y-ERYB-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles/.p>Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 832-10/84-Y-ERM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 832-35/1-Y-ERYB-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 833-10/84-Y-ERYM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 834-35/1-Y-ERA-LMP Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 838-10/182-Y-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 890-25/1-CR-IS Natural PVC Compound Flame retardant and oil resistant PVC compound, recommended for thin wall insulation of automotive electrical wires for working at the temperature range of -40°C to 105°C.Information provided .. |
|||
Specific Gravity | 1.35 - 1.45 g/cc | 1.35 - 1.45 g/cc | ASTM D792 |
Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.41 - 1.45 g/cc | 1.41 - 1.45 g/cc | ASTM D-792 |
Axiall 7800 Moldings & Extrusions Flexible PVC General purpose, 60°C rated molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.41 - 1.45 g/cc | 1.41 - 1.45 g/cc | ASTM D-792 |
Axiall 22850 Coax & Telecom Flexible PVC Flexible PVC jacketing compound for coaxial cable and other 75C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.41 - 1.45 g/cc | 1.41 - 1.45 g/cc | ASTM D-792 |
Axiall 384FR Wire & Cable Flexible PVC Highly flame retardant jacketing compound recommended for direct burial applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.41 - 1.45 g/cc | 1.41 - 1.45 g/cc | ASTM D-792 |
Axiall 8747 Moldings & Extrusions Flexible PVC Economical general purpose molding and extrusion compound with good flex whitening resistance especially in darker colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation i.. |
|||
Specific Gravity | 1.41 - 1.45 g/cc | 1.41 - 1.45 g/cc | ASTM D-792 |
Axiall 12840 Coax & Telecom Flexible PVC Non-lead stabilized CATV coaxial cable jacket. Also suitable for CL2 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 0.950 - 1.45 g/cc | 0.950 - 1.45 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | NBR NM-IEC 60811-1-3 |
Karina 40/130-FC-LMP (SDB) Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |