Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable WJJC32L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
PolyOne Geon™ CPVC EC900 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC900 CPVC is an extrusion compound for CTS Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC900 demonstrates eas.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
PolyOne Geon™ CPVC EC950 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC950 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC950 demonstra.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | |
Sylvin Technologies 9812A-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Techmer ES Plaslube® AC-80/TF/10 NAT Acetal (POM) Copolymer |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® 732E PBT 30% glass/mineral reinforced, excellent thermal performance, low shrinkage and warp. Easy flow.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® GFPC 5040 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Specific Gravity | 1.51 g/cc @Temperature 22.8 °C |
1.51 g/cc @Temperature 73.0 °F |
ASTM D792 |
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |