Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.48 - 1.54 g/cc | 1.48 - 1.54 g/cc | ASTM D 792 |
Karina 806-48/1-BY-ERYB Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.48 - 1.54 g/cc | 1.48 - 1.54 g/cc | ASTM D 792 |
Karina E 45/56-GEN Gold MBATCH (SP31447) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.50 - 1.54 g/cc | 1.50 - 1.54 g/cc | ASTM D-792 |
Axiall 22460 Coax & Telecom Flexible PVC Non-lead stabilized, 75C rated PVC riser jacket over HDPE. Recommended minimum jacket thickness of 22 mils.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.50 - 1.54 g/cc | 1.50 - 1.54 g/cc | ASTM D-792 |
Axiall 8770 Moldings & Extrusions Flexible PVC General purpose extrusion compound for weatherstrips, tubings and gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |