Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Quantum Composites AMC™ 2593 45% Carbon Fiber Reinforced Phenolic SMC AMC™ 2593 (126-40-139) is a carbon fiber reinforced phenolic engineered structural composite molding compound. The carbon fiber is PAN based 3K standard modulus tow. It exhibits outstanding low f.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | |
Resin Technology Group KONA 871 Low Cost Epoxy Resin Mix ratio 100 to 25 by weight.Kona 871 is a low cost epoxy resin system developed for production casting, potting, encapsulating and coating applications where easy handling, good flowability and lo.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | Method A; ASTM D792 |
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of .. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
GEHR Plastics Corzan® PVC-C Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Loxim 330 01V0 Nylon 6 Information provided by Loxim Industries |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-0797 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-0904/GN PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d.. |
|||
Specific Gravity | 1.55 g/cc @Temperature 23.0 °C |
1.55 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183/1 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Specific Gravity | 1.55 g/cc @Temperature 25.0 °C |
1.55 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® LS 4-9080 FLUOROSILICONE RUBBER Information provided by Dow Corning |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
E-Polymers SEPAZ® V240A 40% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Asahi Glass AFLAS® 100S TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Asahi Glass AFLAS® 150E TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Specific Gravity | 1.55 - 1.65 g/cc | 1.55 - 1.65 g/cc | Natural; ASTM D-792 |
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |