Polymer Property : Specific Gravity = 1.56 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.52 - 1.56 g/cc
1.52 - 1.56 g/cc
ASTM D 792
Karina Karintox ENCH./03 Polyolefin Compound
Karintox is a thermoplastic polyolefin, flame retardant, non-halogen, and low smoke emission. Recommended for electrical coating for cables until 1KV. For a better usage/processing, a pre-warm/heat ..
Specific Gravity 1.50 - 1.56 g/cc
1.50 - 1.56 g/cc
NBR NM-IEC 60811-1-3
Karina 42/6-FC-LMP Red Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.50 - 1.56 g/cc
1.50 - 1.56 g/cc
NBR NM-IEC 60811-1-3
Karina E 42/6-FC-LMP Red Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
Specific Gravity 1.50 - 1.56 g/cc
1.50 - 1.56 g/cc
ASTM D 792
Karina E 800-18/695-CY-RT-PO Compound PVC Gray
Rigid PVC compound dry blend, recommended for extrusion of discharge pipes/tubes.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.52 - 1.56 g/cc
1.52 - 1.56 g/cc
after injection; ASTM D792
Compuestos Dominicanos Polycom CE-053175-01 PVC Compound
Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist..
Specific Gravity 1.52 - 1.56 g/cc
1.52 - 1.56 g/cc
ASTM D-792
Axiall 02890 Plenum Flexible PVC
Non-lead stabilized PVC plenum jacket compound recommended for Category 5 applications. Good flexibility and handling during installation.Information provided by Georgia GulfGeorgia Gulf became Axi..
Specific Gravity 1.50 - 1.56 g/cc
1.50 - 1.56 g/cc
ASTM D 792
Karina 800-36/395-CY-RT Brown PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.