Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-20 CRSX Polyester SMC Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-15 CRSX Polyester BMC Premi-Glas® 2103-15 CR-SX is a 15% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Specific Gravity | 1.79 - 1.85 g/cc | 1.79 - 1.85 g/cc | ASTM D 792 |
Karina 18/268-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers. |