Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-10 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-22 CRSX Polyester BMC Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Specific Gravity | 1.80 - 1.85 g/cc | 1.80 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 1.80 - 1.85 g/cc | 1.80 - 1.85 g/cc | ASTM D792 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.75 - 1.85 g/cc @Thickness 1.57 mm |
1.75 - 1.85 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Specific Gravity | 1.79 - 1.85 g/cc | 1.79 - 1.85 g/cc | ASTM D 792 |
Karina 18/268-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
BCC Products METAL-KAST BC 8010 Urethane Casting New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to.. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Bulk Molding Compounds BMC 810 General Purpose Molding Compound BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel.. |