Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC1000 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca.. |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC1100 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca.. |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC1101 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca.. |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC2100 Double-Wall Isolated and Bundled Carbon Nanotubes - Research Grade NANOCYL™ NC2000 series double-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 90% ca.. |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC2101 Double-Wall Isolated and Bundled Carbon Nanotubes - Research Grade NANOCYL™ NC2000 series double-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 90% ca.. |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC3100 Thin Multi-Wall Carbon Nanotubes - Research Grade NANOCYL™ NC3000 series thin multi-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 95.. |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC3101 Thin Multi-Wall Carbon Nanotubes - Research Grade NANOCYL™ NC3000 series thin multi-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 95.. |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC7000 Thin Multi-Wall Carbon Nanotubes NANOCYL™ NC7000 Series, thin multi-wall carbon nanotubes, are produced via the catalytic carbon vapor deposition (CCVD) process.These carbon nanotubes are unique and prized world-wide because their.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | |
P & P Technology Conductive Elastomer Nickel Graphite particlesInformation provided by P & P Technology |
|||
Specific Gravity | 1.60 - 2.00 g/cc | 1.60 - 2.00 g/cc | |
Parker Chomerics CHO-SHIELD® 4076 Conductive Coating CHO-SHIELD® 4076 nickel-filled polyurethane is recommended for shielding an entire room. This durable coating adheres well to plaster, wood, glass, concrete, drywall and most metals.Information pro.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Parker Chomerics CHO-SHIELD® 4916 Conductive Coating Conductive CoatingInformation provided by Chomerics |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ASTM D792 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ASTM D792 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.70 - 2.00 g/cc | 1.70 - 2.00 g/cc | IEC 1212-2 8.1 |
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | IEC 1212-2 8.1 |
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinfo.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Parker Chomerics CHO-BOND 1035 Electrically Conductive Sealant Electrically conductive, one component RTV silicone which provides both environmental sealing and EMI/RFI shielding. This sealant, filled with silver-plated glass particles, contains no acetic acid,.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |