Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 2.15 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.65 - 2.15 g/cc
1.65 - 2.15 g/cc
Base Material; ASTM D792
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Specific Gravity 1.65 - 2.15 g/cc
1.65 - 2.15 g/cc
ASTM D792
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer
Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R..
Specific Gravity 1.65 - 2.15 g/cc
1.65 - 2.15 g/cc
Parker Chomerics CHO-SEAL E6306 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Specific Gravity 1.65 - 2.15 g/cc
1.65 - 2.15 g/cc
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Specific Gravity 1.95 - 2.15 g/cc
1.95 - 2.15 g/cc
ISO 1183
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
Specific Gravity 1.65 - 2.15 g/cc
1.65 - 2.15 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer
Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics
Specific Gravity 2.09 - 2.15 g/cc
2.09 - 2.15 g/cc
ASTM D 792
Karina 1100/1075 IE MBPP White Color Concentrate
Filled white concentrate recommended for olefin applications. Recommended usage from 5%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Copyright © lookpolymers.com All Rights Reserved