Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 3.5 cSt | 3.5 cSt | |
ChevronTexaco Oil Rust Proof Texaco Rust Proof Oil delivers value through:Good short-term rust protection — Low viscosity oil provides complete coverage of metal surfaces for maximum protection against oxidation and corrosion... |