Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1100 cP @Temperature 160 °C |
1100 cP @Temperature 320 °F |
Rheology, 2°C/min |
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character.. |
|||
Viscosity | 1100 cP @Temperature 25.0 °C |
1100 cP @Temperature 77.0 °F |
Adhesive (cp #40, 20 rpm) |
Tra-Con Tra-Coat CF103B UV Curable Rigid Coating TRA-COAT CF103B is a high-gloss, UV curable polymer coating. It provides a wear layer with outstanding gloss retention, moisture resistance, stain resistance, and abrasion resistance. It can be used.. |
|||
Viscosity | 1100 cP @Temperature 75.0 °C |
1100 cP @Temperature 167 °F |
A Side |
ACC EP AEP EPI Engineered Polymers EP AEP is a new generation of Internetwork Polymers of polyurea and Epoxy, “Powered by Reactamine® Technology”. EP AEP was developed for a colorfast floor for both residential and industrial appl.. |