Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 250 cP @Shear Rate 10.0 1/s, Temperature 290 °C |
250 cP @Shear Rate 10.0 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Viscosity | 250 cP @Shear Rate 10.0 1/s, Temperature 290 °C |
250 cP @Shear Rate 10.0 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 250 cP @Shear Rate 10.0 1/s, Temperature 290 °C |
250 cP @Shear Rate 10.0 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 250 cP @Temperature 54.5 °C |
250 cP @Temperature 130 °F |
|
BASF Pluracol® 1538 Slabstock Foam Polyol Description: Pluracol® 1538 polyol is intended for the production of Visco-Elastic foam typically formulated with another base product such as Pluracol 593 polyol. The combination of these two immi.. |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
|
BASF Pluracol® P2010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |