Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3262R PC (Asia Pacific) Lexan* 3262R Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V2@1.5mm rating and is available .. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Pocan® ECO T 3215 000000 PBT + PET, 15% Glass Fiber PBT + PET, 15% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | |
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | |
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon AE004E ABS LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region... |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO 294-4 |
Styron CALIBREâ„¢ 7100-8 Polycarbonate CALIBREâ„¢ 7100-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL IGN320 PPE+PS 20% glass reinforced PPE + PS. High heat, high modulus automotive applications like ignition coils. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0070 cm/cm | 0.0020 - 0.0070 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70 Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70 Product description: Grivory GVX-7H natural is a 70% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)
(Unverified Data**) 55% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Low Warpage and High Stiffness Zytel HTNFR55G50NHLW BK046 is a 50% glass reinforced flame retardant high perf.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | |
E-Polymers SEPAZ® LB60 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific) LNP STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |