Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Asia Pacific) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP COLORCOMP AX98567H ABS LNP* COLORCOMP* AX98567H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | Normal (DAM); ISO 294-4 |
DSM Akulon® K224-G8U (Cond.) 43% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | |
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0070 cm/cm @Time 86400 sec |
0.0040 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE0049F PC LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding... |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 1.50 - 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 1760 PBT+PC 11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 4.00 mm |
0.0040 - 0.0060 in/in @Thickness 0.157 in |
|
Teijin Multilon TN-7000F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness realizes the thin wall of business machine chassis.Information provided by Teijin Chemicals Ltd. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 4.00 mm |
0.0040 - 0.0060 in/in @Thickness 0.157 in |
|
Teijin Panlite® BN-8110R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 4.00 mm |
0.0040 - 0.0060 in/in @Thickness 0.157 in |
|
Teijin Panlite® GS-3410 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | LATI |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |