Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
Polyplastic Armlen® PP MF 40-4M Polypropylene Copolymer, 40% Calcium Carbonate High impact resistance at low temperatureInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latilub 66-20T G/20-V1 PA66, 20% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latiohm 82-02 PD09 PA12 Semiconductive/dissipative product based on Polyamide 12 (PA12). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
LATI Latiohm 83-07 PD11 CNT PA12, Impact Modified Semiconductive/dissipative product based on Polyamide 12 (PA12), impact modified. Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.012 cm/cm | 0.011 - 0.012 in/in | mold temp=100°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.012 cm/cm @Thickness 3.20 mm |
0.0070 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA 30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1398 BK12 30% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF25-66 XE-NBK1 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® GF33-66/6 XE-BKDX9 Nylon 66/6, 33% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® GFT33N051-NBK2 Nylon 66, 33% Glass Fiber Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6 Description: Glass Fiber Reinforced, Lubricated Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® MRGF25/15 42H-BKJA6A Nylon 6, 25% Mineral and 15% Glass Reinforced Ford JA6A color matchedAll information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF25/15 42H-GY1 40% Mineral/Glass Fiber Reinforced Nylon 6 Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® MRGF30/10 42H-GY1 Nylon 6, 30% Mineral and 10% Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latilub 66-15ST G/30 PA66, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.18 mm |
0.010 - 0.012 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |