Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.012 - 0.014 cm/cm @Thickness 3.18 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.014 cm/cm @Thickness 3.18 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.014 cm/cm | 0.0105 - 0.014 in/in | |
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.014 cm/cm | 0.0115 - 0.014 in/in | |
LATI Latamid 6 BH PA 6, Heat Stabilized Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | |
LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced Polyoxymethylene (POM) based compound. Glass fibers. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | |
LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | |
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.014 cm/cm | 0.0115 - 0.014 in/in | |
LATI Latistat 62-08 PA6 Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.014 cm/cm @Thickness 3.18 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.014 cm/cm @Thickness 3.18 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.014 cm/cm @Time 86400 sec |
0.0070 - 0.014 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ISO DIS 294-4 |
Wellman EcoLon® MRGF1619-WBK1 Mineral and Glass Reinforced Recycled Nylon 66 Description: Post Consumer Nylon Compound; WeatherableInformation provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1398-N1 30% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® MR410 22H-WBK 40% Mineral Reinforced, Weatherable Black Nylon 66 Description: Mineral Reinforced, Weatherable Black Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri.. |