Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | ISO Data (Dry) |
BASF Capron® 8202C HS Nylon 6 (Conditioned)
(discontinued **) Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Latistat 45/7-02 HDPE Dissipative product based on High density polyethylene (HD-PE). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.025 cm/cm @Time 86400 sec |
0.015 - 0.025 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP YP003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YP003 is a compound based on Polyester Elastomer containing PTFE, Silicone. Added features include; Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
|
Unitika A1025NO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LHI6 XE-NBK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | ISO 294-4 |
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | |
Eurotec® Tecomid® NB40 NL IH PA 6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm @Thickness 2.00 mm |
0.015 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**) Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | Eurotec |
Eurotec® Tecomid® NA40 NL IX PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.015 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7233 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 8027 POM Copolymer, 30% mineral reinforced POM-MD30Information provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | ISO 2577 |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | Sheet |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Latimass 53/11-02 D030 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | |
Solvay TECHNYL® 1015CR PA6, DRY Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |