Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.017 - 0.029 cm/cm @Thickness 3.17 mm |
0.017 - 0.029 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0470 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | |
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1006D-H31 Nylon Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.026 cm/cm @Thickness 3.20 mm |
0.017 - 0.026 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | Sim. To ISO 294-4 |
DSM Stanyl® TS250FK33 PA46-(GF+MF)30 FR 30% Glass/Mineral Reinforced, Flame Retardant, Low Warpage |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® ST820 BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 BK503 is an unreinforced Super Tough black polybutylene terephthalate resin for injection molding.Information p.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin 100TL is a high viscosity acetal homopolymer containing 1.5% Teflo.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | plate with film gate 150x150x3mm<sup>3</sup> |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | Sheet |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | MPC method |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | MPC method |
Mitsui TPX® RT18 XB Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 3.20 mm |
0.017 in/in @Thickness 0.126 in |
|
Unitika BV2120 PA66, Flame Retardant, Conditioned Information provided by Unitika Ltd. |